Inspection defect guide

Severity and extent codes

Severity

  1. 1As new condition or defect has no significant effect on the element (visually or functionally)
  2. 2Early signs of deterioration, minor defect or damage, no reduction in functionality of element
  3. 3Moderate defect or damage, some loss of functionality could be expected
  4. 4Severe defect or damage, significant loss of functionality and/or element is close to failure or collapse
  5. 5The element is non-functional or failed

Extent

  1. ANo significant defect
  2. BSlight, not more than 5% of surface area, length or number
  3. CModerate, 5% to 20% of surface area, length or number
  4. DWide, 20% to 50% of surface area, length or number
  5. EExtensive, more than 50% of surface area, length or number

1 Metalwork4

1.1

Rusting

Corrosion of steel or iron where the protective coating has broken down

Look forOrange-brown staining, flaking scale and pitting, worst at bottom flanges, connections and areas kept wet by leaking joints or drainage

  1. 1No signs of rusting or damage
  2. 2Minor surface rusting
  3. 3Moderate pitting
  4. 4Deep pits and perforations (localised severe corrosion)
  5. 5Disintegrated by corrosion mechanisms
Report an issue
1.2

Section loss

Loss of metal thickness from advanced corrosion

Look forLaminated (pack) rust, thinned flanges and webs, holes and perforations. Measure remaining thickness against the original section

  1. 1No section loss
  2. 2Minor section loss (penetration less than 5% of section)
  3. 3Moderate section loss causing some reduction in functionality (penetration 5 to 20% of section thickness)
  4. 4Major section loss causing significant reduction in functionality (penetration more than 20% of section)
  5. 5Collapsed or collapsing
Report an issue
1.3

Rusting or damage to bolts

Corrosion, loosening or loss of bolts, nuts, washers and rivets at connections

Look forLoose or missing nuts, wasted rivet heads, rust streaks from bolt holes and cracks through bolts. Separate structural from non-structural fixings

  1. 1No signs of rusting or damage to bolts, nuts or rivets
  2. 2Non structural bolts loose, minor corrosion of nuts and washers
  3. 3Non structural bolts missing, moderate corrosion of rivet heads, nuts and washers
  4. 4Structural bolts missing, rivets loose or missing, crack through bolt
  5. 5Failure of element due to missed/failed bolts/rivets
Report an issue
1.4

Damage to weld

Corrosion of weld runs or fatigue cracking at the weld

Look forCracks at the weld toe or along the weld, often at stiffener ends and welded attachments. Cracked paint over a weld is an early sign

  1. 1No corrosion or damage of weld runs
  2. 2Slight corrosion of weld run
  3. 3Crack at toe of weld, moderate reduction in size of weld due to corrosion
  4. 4Longitudinally cracked weld, major reduction in size of weld due to corrosion
  5. 5Weld connection failure (longitudinal crack)
Report an issue

2 Reinforced and prestressed concrete5

2.2

Spalling

Concrete broken away from the surface, usually pushed off by corroding reinforcement, impact or frost

Look forBroken edges and exposed links or main bars at soffits, arrises and below leaking joints. Note bar corrosion and depth of the spall

  1. 1No spalls
  2. 2Minor localised spalls exposing shear links
  3. 3Major localised spalls exposing shear links and main bars with general corrosion
  4. 4Joined up, deep spalls exposing shear links and main bars with general pitting corrosion
  5. 5Collapsed
Report an issue
2.3

Cracking

Cracks from flexure, shear, shrinkage, thermal movement, settlement or reinforcement corrosion

Look forWidth (crack gauge), length, pattern and orientation. Vertical cracks in tension zones suggest flexure, diagonal cracks near supports suggest shear and cracks along bars suggest corrosion

  1. 1Hairline cracks, difficult to detect visually
  2. 2Cracks and crazing in areas of low flexural behaviour (cracks less than 0.3mm)
  3. 3Cracks and crazing in areas of high flexure (cracks approx 1mm and easily visible)
  4. 4Wide/deep cracks (more than 2mm), shear cracks
  5. 5Element unable to function due to structural cracks
Report an issue
2.4

Prestressing damage

Deterioration of prestressing tendons, ducts or anchorages, often from voids in the duct grout that let water and chlorides reach the strand

Look forCracks along duct lines, rust staining or damp along tendon routes, distress at anchorages and exposed or broken strands

  1. 1No signs of damage to prestressing
  2. 2Substandard grouting of ducts (may not be visible)
  3. 3Cracks along line of prestressing duct
  4. 4Exposed prestressing cable
  5. 5Failed prestressing cables
Report an issue
2.5

Delamination

Separation of the cover concrete along the plane of the reinforcement, the stage before a spall

Look forHollow sound when tapped with a hammer, cracks with rust staining and a slightly raised surface. Mark out the hollow area

  1. 1No signs of delamination
  2. 2Early signs of delamination e.g. cracks with rust staining
  3. 3Delamination in areas of low flexural and/or shear action
  4. 4Delamination in areas of high flexural and/or shear action
  5. 5Failure due to delaminated bars
Report an issue
2.6

Freeze thaw

Surface damage from repeated freezing of water in the pores (freeze-thaw) or sulfate attack forming thaumasite in cold wet conditions

Look forScaling, map cracking and loss of surface on exposed and splash-zone concrete. Soft, white, mushy concrete below ground suggests thaumasite

  1. 1No signs of thaumasite or freeze-thaw attack
  2. 2Slight cracking caused by thaumasite or freeze-thaw
  3. 3Moderate thaumasite or freeze-thaw attack
  4. 4Major thaumasite or freeze-thaw attack
  5. 5Failure due to thaumasite or freeze-thaw attack
Report an issue

3 Masonry, brickwork and mass concrete7

3.1

Deformation

Change of shape of a masonry element, such as a flattened arch profile or distorted courses

Look forSagging or flattened arch crown, kinks in courses and out-of-line string courses and parapets. Sight along the arch from the springing

  1. 1No evidence of deformation
  2. 2Minor deformation
  3. 3Moderate deformation
  4. 4Major deformation
  5. 5Collapsed
Report an issue
3.2

Pointing

Loss or deterioration of the mortar between bricks or stones

Look forRecessed, crumbling or missing joints, plants in joints and loose units. Probe the joints to estimate the depth of loss

  1. 1Pointing sound
  2. 2Minor depth of pointing deterioration
  3. 3Moderate to significant depth of pointing loss, but does not appear to be rapidly disintegrating or crumbling, bricks not easily loosened
  4. 4Pointing very poor condition, severely weathered, crumbling to touch and/or significant depth loss, bricks easily loosened
  5. 5Collapsed
Report an issue
3.3

Arch ring damage

Separation between the rings of a multi-ring brick arch (ring separation)

Look forCracks between rings visible at the arch faces, dropped rings and a drummy sound when the soffit is tapped

  1. 1No arch ring cracking or separation
  2. 2Arch ring cracks difficult to see
  3. 3Arch ring separation (gap less than 25mm)
  4. 4Arch ring separation (gap greater than 25mm)
  5. 5Disintegrated
Report an issue
3.4

Arch barrel crack

Cracking through the arch barrel

Look forLongitudinal cracks (parallel to the span) suggest spreading or a separating spandrel, diagonal cracks near the faces suggest differential settlement and lateral cracks suggest hinging

  1. 1No arch barrel cracks
  2. 2No diagonal cracks, longitudinal cracks less than 3mm wide, lateral cracks
  3. 3Diagonal cracks, longitudinal cracks greater than 3mm wide
  4. 4Diagonal cracks, longitudinal cracks breaking barrel into 1m sections or less
  5. 5Arch barrel failure
Report an issue
3.5

Cracking

Cracks and spalls in masonry and mass concrete away from the arch barrel

Look forStepped cracks along the joints, cracked units, crazing and spalled faces. Record width and whether the crack runs through the units or the joints

  1. 1No cracks
  2. 2Minor hairline cracks and shallow spalls
  3. 3Moderate cracks (easily visible, crazing) and deep localised spalls
  4. 4Major cracks and spalling
  5. 5Failure due to structural cracks
Report an issue
3.6

Section loss

Loss of bricks or stones from the face, or wasting of the units by weathering

Look forMissing units, eroded or frost-spalled brick faces and hollows behind the face

  1. 1No bricks/masonry blocks missing, minor surface weathering
  2. 2Few bricks/stones missing (no adjacent ones missing), major surface weathering
  3. 3Moderate loss of bricks/stones
  4. 4Severe loss of bricks/stones
  5. 5Failure due to missing bricks/stones
Report an issue
3.7

Bulging or leaning

Outward movement of spandrel, wing or retaining walls, often from fill pressure or water behind the wall

Look forBulges, out-of-plumb faces and a crack or gap where the spandrel wall meets the arch ring. Check with a plumb line or level

  1. 1No bulging, leaning or displacement
  2. 2Minor bulging, leaning or displacement
  3. 3Moderate bulging, leaning or displacement
  4. 4Severe bulging, leaning or displacement
  5. 5Collapsed or non-functional
Report an issue

4 Paintwork and protective coatings1

4.1

Coating damage

Breakdown of paint, galvanising or other protective coating systems

Look forChalking, blistering, flaking and chips that expose the undercoat or bare metal, and rust breaking through the finish

  1. 1Finishing coat sound, slight weathering
  2. 2Normal weathering of finishing coat
  3. 3Spot chips and cracks on finishing coat, undercoat exposed but sound
  4. 4Failure of finishing coat and spot chips and cracks to undercoat/substrate
  5. 5All coats failed
Report an issue

5 Vegetation2

5.1

Structural damage

Plants growing on or near the structure, with roots opening joints and cracks

Look forTrees and shrubs rooted in walls, joints and drainage, roots displacing units and large trees close to abutments and wing walls

  1. 1Slight to no vegetation
  2. 2Minor vegetation causing no structural damage (surface mosses, small grass and weeds)
  3. 3Vegetation growth on or near bridge causing structural damage and/or deformation e.g. roots and branches of nearby trees, small trees/plants growing on structure
  4. 4Vegetation growth on or near bridge causing major structural damage and/or deformation e.g. roots and branches of nearby trees, large tree growing on structure
  5. 5Failure caused by vegetation growth or tree collapsing on structure
Report an issue
5.2

Inspection obstruction

Vegetation covering elements so they cannot be inspected

Look forIvy, brambles and undergrowth over faces, bearings and wing walls. Record which elements could not be seen

  1. 1Slight to no vegetation
  2. 2Low depth/density of vegetation cover, easily removed e.g. moss
  3. 3Significant depth/density of vegetation, obscuring inspection e.g. ivy
  4. 4Inspection impossible due to vegetation growth but structural damage due to vegetation unlikely
  5. 5Inspection of critical structural elements not possible due to density of vegetation and root systems likely to be causing structural damage
Report an issue

6 Foundations6

6.1

Settlement

Vertical movement of the foundation

Look forDips in the deck or parapet line, tapering cracks in the substructure and gaps opening under bearings

  1. 1No visible settlement of structure
  2. 2No visible settlement, but cracks may be due to it
  3. 3Minor settlement of structure
  4. 4Major settlement of structure
  5. 5Collapse due to settlement
Report an issue
6.2

Differential movement

Unequal movement between parts of the structure

Look forSteps in parapets and copings and cracks at the junction between wing walls and abutments

  1. 1No visible differential movement of structure
  2. 2No visible movement, but cracks may be due to it
  3. 3Minor differential movement of structure
  4. 4Major differential movement of structure
  5. 5Collapsed due to differential movement
Report an issue
6.3

Sliding

Horizontal movement of a substructure, usually pushed by the retained soil

Look forClosing deck joint gaps, an abutment displaced forward and cracks near the base

  1. 1No visible sliding of structure
  2. 2No visible sliding, but cracks may be due to it
  3. 3Minor sliding of structure
  4. 4Major sliding of structure
  5. 5Collapsed due to sliding
Report an issue
6.4

Rotation

Tilting of an abutment, pier or wall about its base

Look forOut-of-plumb faces, tapering joint gaps and cracks opening at the top or the toe

  1. 1No visible rotation of structure
  2. 2No visible rotation, but cracks may be due to it
  3. 3Minor rotation of structure
  4. 4Major rotation of structure
  5. 5Collapsed due to rotation
Report an issue
6.5

Scour

Removal of bed material from around foundations by flowing water

Look forExposed or undermined footings and hollows at pier noses and abutments, especially after a flood. Probe the bed where it can be reached safely

  1. 1No scour
  2. 2Minor scour
  3. 3Moderate scour
  4. 4Major scour
  5. 5Dangerous scour or failure
Report an issue
6.6

Foundation faults

Defects in the foundation itself, such as a deteriorated footing, piles or timber grillage

Look forCracks in the substructure that trace back to the foundation and exposed or decayed piles

  1. 1Substructure appears unaffected by foundation faults (assume no foundation faults)
  2. 2Foundation faults causing minor cracks in substructure
  3. 3Foundation faults causing moderate cracks in substructure
  4. 4Foundation faults causing major cracks and deformation in substructure
  5. 5Failure due to foundation faults
Report an issue

7 Invert, apron and river bed2

7.1

Scour

Loss of invert, apron or river bed material

Look forHoles or missing stones in aprons, undermined invert edges and a step down where the bed has lowered

  1. 1No scour
  2. 2Minor scour
  3. 3Moderate scour
  4. 4Major scour
  5. 5Dangerous scour or failure
Report an issue
7.2

Vegetation or silt

Silt, debris and plant growth in the channel

Look forSilt build-up reducing the waterway, debris trapped against piers and vegetation in the channel

  1. 1No vegetation growth or silting
  2. 2Vegetation growth, trapped debris and silting causing slight disruption to flow
  3. 3Vegetation growth, trapped debris and silting significant disruption to flow causing faster flow in areas of the river
  4. 4Vegetation growth, trapped debris and silting severe disruption to flow causing much faster flow in areas of the river
  5. 5Failure caused by vegetation growth, trapped debris and silting
Report an issue

8 Drainage4

8.1

Blockage

Drainage partly or fully blocked

Look forStanding water on the deck, silted gullies and blocked pipes. Estimate the share of the cross-section that is blocked

  1. 1In sound condition and fully functional
  2. 2Mostly functional (less than 25% of cross section blocked)
  3. 3Partly functional (25 to 50% of cross section blocked)
  4. 4Mostly non-functional (more than 50% of cross section blocked)
  5. 5Totally blocked/non-functional/broken
Report an issue
8.2

Causing stains

Water from the drainage discharging onto the structure

Look forStaining, leaching and calcite below outlets and pipes

  1. 1Causing no staining
  2. 2Causing minor staining
  3. 3Cleaning of staining required
  4. 4Urgent cleaning required
  5. 5Urgent and frequent cleaning
Report an issue
8.3

Structural damage

Leaking or misdirected drainage causing deterioration of the structure

Look forCorroded steel or spalled concrete below leaking pipes, outfalls and gullies

  1. 1No structural damage
  2. 2Causing minor structural damage
  3. 3Causing structural damage
  4. 4Causing major structural damage
  5. 5Causing severe damage to adjacent elements
Report an issue
8.4

Weep hole blockage

Weep holes and outlets blocked, trapping water behind walls

Look forDry weep holes after rain, plants or silt in the holes and damp patches on the face

  1. 1No blockage of weep holes, outlets
  2. 2Minor blockage of weep holes, outlets
  3. 3Moderate blockage of weep holes, outlets
  4. 4Major blockage of weep holes, outlets
  5. 5Non-functioning weep holes
Report an issue

9 Surfacing6

9.1

Wear and weathering

Loss of surface material from traffic and weather

Look forPolished aggregate, loss of fines and a worn, ravelled surface

  1. 1Little to no wear and weathering
  2. 2Minor wear/weathering
  3. 3Moderate wear/weathering
  4. 4Major wear/weathering
  5. 5Dangerous
Report an issue
9.2

Crazing, tracking & fretting

Crazing (fine cracks), tracking (rutting in the wheel paths) and fretting (loss of aggregate)

Look forRuts in the wheel paths, loose chippings and a network of fine cracks

  1. 1No crazing, tracking or fretting
  2. 2Minor crazing, tracking and/or fretting
  3. 3Moderate crazing, tracking and/or fretting
  4. 4Major crazing, tracking and/or fretting
  5. 5Complete break up
Report an issue
9.3

Poor texture

Surface texture too open or poorly compacted, letting water down to the deck

Look forOpen, porous surface with visible voids, compared with a dense well-closed surface

  1. 1Dense
  2. 2Poor texture
  3. 3Open texture
  4. 4Very open texture
  5. 5Dangerous
Report an issue
9.4

Cracking

Cracks in the surfacing, often reflecting joints or movement in the deck below

Look forTransverse cracks over supports and joints, longitudinal cracks and break-up of the top layer

  1. 1Sound
  2. 2Cracks in top layer
  3. 3Top layer breached
  4. 4Deep cracks and potholes
  5. 5Top layer completely missing
Report an issue
9.5

Slippery

Loss of skid resistance

Look forPolished, smooth or contaminated surfaces, especially on footways, ramps and steps

  1. 1Not slippery
  2. 2Starting to become slippery
  3. 3Definitely becoming slippery
  4. 4Slippery
  5. 5Dangerous
Report an issue
9.6

Cracked flagged surfacing

Cracked, rocking or displaced paving flags creating trip hazards

Look forCracked and missing flags and trip heights. Measure the largest trip

  1. 1No defects
  2. 2Trips <5mm
  3. 3Cracked flags, trips >5mm and <10mm
  4. 4Trips >10mm and <20mm
  5. 5Trips >20mm
Report an issue

10 Expansion joints12

10.1

Asphaltic plug debonding

An asphaltic plug joint separating from the adjacent surfacing

Look forOpen gaps along one or both edges of the plug

  1. 1Sound
  2. 2Minor debonding between plug and road
  3. 3Moderate debonding between plug and road
  4. 4Major debonding between plug and road
  5. 5Dangerous
Report an issue
10.2

Asphaltic plug material loss

Loss of binder and aggregate from an asphaltic plug joint

Look forExposed or loose aggregate, a ravelled plug surface and potholes in the plug

  1. 1Sound
  2. 2Slight loss of surface binder and aggregate
  3. 3Loss of aggregate (surface penetration 20 to 50mm)
  4. 4Loss of material from joint (causing holes >50mm deep)
  5. 5Missing
Report an issue
10.3

Asphaltic plug tracking

Binder flowing and the plug rutting under traffic, worst in hot weather

Look forWheel ruts in the plug and binder pushed up at the edges

  1. 1Sound
  2. 2Minor tracking and flow of binder
  3. 3Moderate tracking and flow of binder
  4. 4Major tracking and flow of binder
  5. 5Disintegrated
Report an issue
10.4

Cracking along nosing

Cracks along the nosings either side of the joint

Look forCracked or broken nosing concrete or resin and loose pieces at the joint edge

  1. 1Sound
  2. 2Minor cracking along nosing
  3. 3Moderate cracking along nosing, some breakup
  4. 4Breakup of nosing material
  5. 5Disintegrated
Report an issue
10.5

Elastomeric and others missing bolts

Fixing bolts missing across a mechanical or elastomeric joint

Look forEmpty bolt holes and plates that rock or rattle under traffic

  1. 1Minor signs of wear
  2. 2One bolt missing at cross section
  3. 3Numerous bolts missing at cross section
  4. 4Majority of bolts missing at cross section
  5. 5Failure due to missing bolts
Report an issue
10.6

Elastomeric and others sealant breached

A strip or compression seal loose, torn or dropped

Look forDropped or pulled-out seals and debris packed into the gap

  1. 1Strip sealant sound
  2. 2Strip sealant loose/poor, compression seal dropped and/or worn
  3. 3Sealant breached, strip sealant breached
  4. 4Sealant missing, strip sealant missing/out
  5. 5Failure
Report an issue
10.7

Elastomeric and others road breaking

Break-up of the road surface next to the joint

Look forPotholes and cracks either side of the joint and debris in the joint

  1. 1Sound road surface adjacent to joint
  2. 2Minor breakup of road surface adjacent to joint
  3. 3Moderate break up of road surface adjacent to joint, some debris in joint seal
  4. 4Major breakup of road surface adjacent to joint, significant debris in joint seal
  5. 5Joint failure due to deteriorated condition of adjacent road surface
Report an issue
10.8

Elastomeric and others loose fixings

Loose fixings or missing bolt sealer

Look forMissing caps or sealer over bolts and fixings that move under traffic

  1. 1Sound fixings
  2. 2Bolt sealer missing
  3. 3Fixings loose
  4. 4Fixings missing, plates and angles loose
  5. 5Failure due to missing fixtures
Report an issue
10.9

Elastomeric and others component damage

Cracking or tearing of joint components

Look forTorn elastomer, cracked steel fingers or plates and broken parts

  1. 1Sound components
  2. 2Initiation of cracking or tearing of components
  3. 3Crack/tear <20% of width of component
  4. 4Crack/tear >20% but <50% of width of component
  5. 5Failure of expansion joint components
Report an issue
10.10

Buried joint cracking

Surface cracking above a buried joint

Look forA crack line in the surfacing directly over the joint

  1. 1Reasonably sound
  2. 2Minor surface cracking
  3. 3Moderate surface cracking
  4. 4Major surface cracking
  5. 5Failure
Report an issue
10.11

Buried joint sealant damage

Breakdown of the sealant in the induced crack above a buried joint

Look forCracked, lost or broken-up sealant along the joint line

  1. 1Sealant for induced crack is sound
  2. 2Minor cracking or breakup of sealant for induced crack
  3. 3Moderate cracking or breakup of sealant for induced crack
  4. 4Major cracking or breakup of sealant for induced crack
  5. 5Disintegrated or missing of sealant for induced crack
Report an issue
10.12

Joint leakage

Water passing through the joint onto the structure below

Look forStaining, damp and calcite on bearing shelves, abutment faces and deck ends under the joint

  1. 1No visible signs of leakage
  2. 2Minor leakage through joint
  3. 3Moderate leakage through joint
  4. 4Major leakage through joint causing structural damage
  5. 5Open joint causing major structural damage
Report an issue

11 Embankments1

11.1

Deformation or settlement

Deformation, subsidence or slips of approach and retained embankments

Look forTension cracks at the crest, bulging at the toe, leaning trees and posts and dips in the road or footway above

  1. 1Sound, no deformation
  2. 2Minor subsidence, minor deformation
  3. 3Minor slip, settlement causing slight cracking of carriageway
  4. 4Major slip/settlement causing major cracking of carriageway
  5. 5Critical slip/settlement
Report an issue

12 Bearings6

12.1

Rusting

Corrosion of steel bearing components

Look forRust on plates, rollers, rockers and guides and debris packed around the bearing

  1. 1Negligible rusting, minor weathering
  2. 2Minor rusting, moderate weathering
  3. 3Moderate rusting
  4. 4Major rusting
  5. 5Failed or seized due to rusting
Report an issue
12.2

Offset or dislodged

A bearing displaced from its correct position

Look forBeam off-centre on the bearing, tilted rockers and plates or pads moved out of line

  1. 1Correct position
  2. 2Minor offset
  3. 3Moderate offset/tilt
  4. 4Dislodged
  5. 5Off bearing/missing
Report an issue
12.3

Sliding

A sliding bearing at a skewed or extreme position for the temperature at the time

Look forCompare the position indicator with the expected position for the air temperature. Note the temperature on the record

  1. 1Sliding bearing in correct position
  2. 2Sliding bearing in slightly skewed (off centre) position at normal temp
  3. 3Sliding bearing at end of travel in normal temperatures
  4. 4Sliding bearing beyond designed extent of travel at normal temperatures
  5. 5Sliding bearing failed
Report an issue
12.4

Crazing

Crazing and breakdown of an elastomeric bearing surface

Look forSurface crazing, external breakdown and bulging of the elastomer

  1. 1No crazing
  2. 2External crazing
  3. 3External breakdown
  4. 4Major breakdown (PTFE, laminations, rubber etc.)
  5. 5Complete breakdown
Report an issue
12.5

Sliding plate damage

Deformation or damage of sliding plates

Look forBent or scored plates and PTFE squeezed out or missing

  1. 1Sliding plate sound
  2. 2Minor deformation of sliding plate
  3. 3Moderate deformation of sliding plate
  4. 4Major deformation of sliding plate
  5. 5Bearing seized by sliding plate deformations
Report an issue
12.6

Bearing damage

Cracking, splitting or disintegration of the bearing

Look forSplit or crushed elastomer, cracked components and a loose bearing

  1. 1Bearings sound
  2. 2Minor cracks
  3. 3Moderate cracks or loose
  4. 4Splitting and deformation
  5. 5Disintegrated
Report an issue

13 Impact damage1

13.1

Impact

Damage from a vehicle, vessel or debris strike

Look forScoring and chipping of beam faces, bricks knocked out of the arch, deformed steelwork and fresh scrape marks on soffit edges. Check the headroom signs

  1. 1No damage
  2. 2Slight surface scoring, minor displacement of element e.g. marking and chipping of beam faces, several bricks across arch barrel width, slight impact deformation of steelwork
  3. 3Moderate displacement of element e.g. beam slightly offset on bearings, significant number of bricks knocked out across arch barrel width, moderate impact deformation of steelwork
  4. 4Severe displacement of element e.g. beam dislodged off bearings, many bricks knocked out across arch barrel width, major impact deformation of steelwork
  5. 5Knocked down, broken, collapsing
Report an issue

14 Waterproofing2

14.1

Non structural damage

Water passing through the deck or arch where the waterproofing has failed

Look forDripping and seepage on the soffit and arch barrel, away from the joints. Leaks through the joints are recorded under expansion joints

  1. 1No visible sign of seepage
  2. 2Minor seepage through deck/arch etc. (slow dripping)
  3. 3Moderate seepage through deck/arch etc. (some resistance to seepage)
  4. 4Major seepage (little resistance) through deck/arch etc. causing structural damage
  5. 5Non-functional, causing critical structural damage
Report an issue
14.2

Structural damage

Damp and staining on the soffit from failed waterproofing

Look forDamp or wet soffits, water stains, calcite and stalactites

  1. 1No visible sign of seepage
  2. 2Damp surface, slight water stains on soffit
  3. 3Wet surface, drops of water falling and significant staining
  4. 4Very wet surface and stalactites causing structural damage
  5. 5Major structural damage caused by waterproofing not functioning properly
Report an issue

15 Stone slab bridges1

15.1

Cracking or displacement

Cracking or displacement of the slabs in a stone slab bridge or culvert

Look forCracked, dropped or displaced slabs and slabs losing their bearing on the walls

  1. 1Sound, no defects or damage
  2. 2Minor cracking
  3. 3Moderate cracking but no visible displacement
  4. 4Major cracking and/or displacement
  5. 5Collapsed
Report an issue

16 Timber2

16.1

Damage

Mechanical damage to timber, such as splits, checks and crushing

Look forSplits along the grain, crushed bearing areas and loose or corroded fixings

  1. 1No sign of damage
  2. 2Minor signs of damage
  3. 3Moderate signs of damage
  4. 4Major signs of damage
  5. 5Disintegrated through damage
Report an issue
16.2

Section loss

Loss of section from rot or insect attack

Look forSoft timber when probed, fungal growth and decay at ends, joints and anywhere water collects

  1. 1No section loss
  2. 2Minor section loss (decay less than 5% of section)
  3. 3Moderate section loss causing some reduction in functionality (decay 5 to 20% of section thickness)
  4. 4Major section loss causing significant reduction in functionality (decay more than 20% of section thickness)
  5. 5Collapsed or collapsing
Report an issue